Garantindo a aplicação correta e eficiente das tecnologias de NDT (Ensaios Não Destrutivos), assegurando a qualidade e a segurança de cada processo.
22/01/2025SINSO Integrated Welding Solutions has been excelling in the validation of its welding procedures, complying with the stringent qualification standards ASME IX and AWS D1.1.
Test Tube: CP-SIS-001
Material: API 5L X52 – DN – 16” – Thickness 12.7mm – T-131291503
Consumable: ER70S-3 / E-7018-1H4R
Welding Process: GTAW + SMAW
Preparation: ASME IX QW 462.1 (b) / AWS D1.1 Ed. 2020 (fig. 6.10)
Test Method: ASME IX QW 152 / AWS D1.1 Ed. 2020 – 6.10.3.1
Acceptance Criteria: ASME IX QW 153 / AWS D1.1 Ed. 2020 – 6.10.3.3
Notch Diameter: Maximum 40mm
Test Method: AWS D1.1 Ed. 2020 – 6.10.3.4
Acceptance Criteria: AWS D1.1 Ed. 2020 – 6.10.3.5
This reflects our ongoing commitment to quality and safety, providing efficient and secure solutions for our clients.
SINSO Integrated Welding Solutions – Garantindo a qualidade em cada solda!